245 |
_aSubcritical crack growth due to fatigue, stress corrosion and creep _blectures from a course held at the Joint Research Centre, Ispra, Italy, October 19th-23rd, 1981 in collaboration with the European Group on Fracture _cedited by L.H. Larsson |
||
260 |
_aLondon _bElsevier _c1984 |
||
300 |
_axiv, 617 s. _bgraf., res. _c24 cm. |
||
504 | _aKaynakça var. | ||
650 | _aFracture mechanics. | ||
650 |
_aMaterials _vCreep. |
||
650 |
_aMaterials _vFatigue. |
||
650 | _aStress corrosion. | ||